South Bow Releases Root Cause Analysis of Keystone Pipeline Rupture

South Bow's analysis reveals Keystone Pipeline rupture caused by fatigue crack in weld from hydrogen brittleness over 15 years. Company implementing enhanced inspections and remedial measures.